Selective Leaching of Silver-Rich Residue in NH4SCN Solution under Oxygen Pressure

Shenghai Yang,Gengtao Chen,Yanan Cai,Huan Guo,Weiyi Yao,Motang Tang
DOI: https://doi.org/10.1016/j.seppur.2010.11.003
IF: 8.6
2011-01-01
Separation and Purification Technology
Abstract:An oxidative pressure leaching process to extract silver from the silver-rich residue of demanganized silver–manganese sulfide concentrate with ammonium thiocyanate solution was investigated in this paper. The effects of several factors: temperature, leaching time, oxygen pressure, Fe3+ concentration, lignin concentration, and initial pH of the leaching reagent, on the extraction percentages of silver were studied. The following optimized leaching conditions were obtained: Fe3+ concentration 4.2g/L, lignin concentration 0.6g/L, NH4SCN concentration 1.5M, initial pH value 1.8, and oxygen pressure 1.4MPa at 120°C for 3h. Under these optimized conditions, the average extraction percentage of silver was about 88% and 6.5% of NH4SCN was lost after four cycles. The ammonium thiocyanate method has advantages over the conventional cyanidation method and chlorination method, with a higher efficiency, lower toxicity and better selectivity and stability.
What problem does this paper attempt to address?