Micron-Bubble Formation on Polycrystal Tungsten Due to Low-Energy and High-Flux Helium Plasma Exposure
D Nishijima,M Miyamoto,H Iwakiri,MY Ye,N Ohno,K Tokunaga,N Yoshida,S Takamura
DOI: https://doi.org/10.2320/matertrans.46.561
2005-01-01
MATERIALS TRANSACTIONS
Abstract:Surface modification of polycrystal tungsten due to low-energy and high-flux helium plasma exposure was investigated. Micron-sized holes and bubbles were formed on the surface at a surface temperature of 2200 K even when the incident ion energy of helium was 10eV. Hole formation was significantly reduced on the surface when the incident ion energy of helium was around 5 eV and no surface modification was seen at less than 5 eV. Coalescence of micron-sized helium bubbles was observed in the cross section of a W sample.