Sulfur Composite Cathode Materials for Rechargeable Lithium Batteries

JL Wang,J Yang,CR Wan,K Du,JY Xie,NX Xu
DOI: https://doi.org/10.1002/adfm.200304284
IF: 19
2003-01-01
Advanced Functional Materials
Abstract:Conductive polymer/sulfur composite materials were prepared by heating the mixture of polyacrylonitrile (PAN) and sublimed sulfur. During the heating process, PAN was dehydrogenated by sulfur, forming a conductive main chain similar to polyacetylene. At the same time, the high-polarity functional group-CN cyclized at the melt state, forming a thermally stable heterocyclic compound in which sulfur was embedded. The nanodispersed composites showed excellent electrochemical properties. Tested as cathode material in a non-aqueous lithium cell based on poly(vinylidene fluoride) (PVDF) gel electrolyte at room temperature, the composite exhibited a specific capacity up to 850 mA h g(-1) in the initial cycle. Its specific capacity remained above 600 mA h g(-1) after 50 cycles, about five times that of LiCoO2, and recovered partly after replacement of the anode with a fresh lithium sheet. The utilization of the electrochemically active sulfur was about 90% assuming a complete reaction to the product, Li2S.
What problem does this paper attempt to address?