Abstract:Three series of ZnO-based varistor materials with different doping levels of Bi2O3 and Sb2O3 were prepared, and their mechanical properties were measured. Under 2%Bi (atomic fraction), with increasing amount of Sb in an appropriate range, the ZnO grain size decreases, the porosity almost has no change, and the relative density increases. As a result, the modulus, bending strength and fracture toughness increase. Under 3%Sb (atomic fraction), with increasing amount of Bi, the grain size and porosity increase, thus the relative density decreases, which results in the decrease of modulus, bending strength and fracture toughness. The optimum ZnO-based composite has elastic modulus of 114 GPa, flexure modulus of 115 GPa, bending strength of 120 MPa, and fracture toughness of 1.87 MPa.m(1/2).
What problem does this paper attempt to address?