Abstract:Iron oxides coated on Fe0 core–shell nanospheres (nIOCI) were synthesized through the reduction of ferrous sulfate aqueous solution by sodium borohydride at ambient atmosphere. The catalyst was highly effective for the degradation of humic acid (HA) in the presence of H2O2 and UVA at neutral pH. Under deoxygenated conditions in the dark, the generation of hydroxyl radicals in aqueous nIOCI dispersion verified its galvanic cell-like performance, which enhanced the interfacial electron transfer and led to its higher reactivity. By the total organic carbon, the absorbance of UV254, FTIR, the molecular weight distribution and the chemical fractional character analysis, the degradation process of HA was shown to proceed by the disappearance of aromaticity, the increase of hydrophilic fraction and aromatic ring openings into CO2 and small organic acid. The treated HA showed much lower reactivity toward chlorine and the disinfection byproduct (DBP) formation potential was also greatly reduced. Moreover, it was found that the DBP formation potential more depended on the structure of the intermediates of HA degradation than TOC removal.
What problem does this paper attempt to address?