Synthesis of Oxidized Starch Adhesive

于海莲,胡震
DOI: https://doi.org/10.3969/j.issn.1004-0935.2008.09.003
2008-01-01
Abstract:Oxidized starch adhesive was prepared by one step oxidation with starch as raw material at normal temperature and atmospheric pressure.The main factors influencing its viscosity were oxidation time,the dosage of water,the dosage of oxidizer,the dosage of plasticizer and pasting agent.The optimal preparation method was chosen as follows: when the dosage of starch used was 25 g,oxidation time was 60 minute,the dosage of water and solution of sodium hypochlorite was 60 and 4 mL respectively,calcium chloride was 0.14 g,and sodium hydroxide was 2.0 g.Viscosity of the adhesive that was prepared according to above-mentioned method could reach 275 MPa·s.