The Effect of Material, Thermal and Laser Conditioning on the Damage Threshold of Type Ii Tripler-Cut Dkdp Crystals

Shao-Tao Sun,Lai-Lin Ji,Zheng-Ping Wang,Ming-Xia Xu,Liang,Bing Liu,Xiao-Ming Mu,Xun Sun,Xin-Guang Xu
DOI: https://doi.org/10.1002/crat.200711129
2008-01-01
Crystal Research and Technology
Abstract:By using the traditional temperature-reduction method, KD2PO4 (DKDP) crystals were grown from 85%-deuterated aqueous solution synthesized by different kind of KH2PO4 (KDP) raw materials. An experimental technique was employed to measure the variation of bulk damage threshold in plates of DKDP crystals. Bulk laser damage in unconditioned, thermal-conditioned and laser-conditioned type II tripler-cut DKDP crystals has been studied using 1064 nm (omega) and 355 nm (3 omega) laser at pulse lengths of 5ns, 5ns respectively. (C) 2008 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.
What problem does this paper attempt to address?