Preparation of Electrospun In_2 O_3 /cdo Composite and Its Formaldehyde-Sensing Properties

Chen Peng-Peng,Wang Jing,Zhang Chun-Li,Hao Yu-Wen,Du Hai-Ying
DOI: https://doi.org/10.3866/pku.whxb201306091
2013-01-01
Abstract:In(NO3)(3)/polyvinyl pyrrolidone (PVP) nanofiber precursors were synthesized using a traditional electrospinning method, and were then annealed at 500, 600, and 700 degrees C to form In2O3 nanofibers. The as-prepared In2O3 nanofibers were characterized using X-ray diffraction (XRD), thermal gravimetry and differential thermal analysis (TG/DTA), and field-emission scanning electron microscopy (FE-SEM). The results show that the In2O3 nanofibers crystallize well, with a small average grain size (about 24 nm) and a good mesoporous structure, when annealed at 500 degrees C. The In2O3 nanofibers annealed at the three temperatures were further used to fabricate gas sensors. The test results show that the sensor based on In2O3 annealed at 500 degrees C has the highest response (about 7) to 10 x 10(-6) (volume fraction, phi) formaldehyde (HCHO) at an operating temperature of 240 degrees C. CdO nanoparticles were also prepared using the same method; XRD and FE-SEM show that the average grain size of CdO is about 68 nm. Finally, the as-prepared In2O3 nanofibers were mixed with the as-prepared CdO in molar ratios of 1:1, 10:1, and 20:1, and the mixtures were used to fabricate gas sensors. The HCHO-sensing properties of the sensors based on pure In2O3 and In2O3/CdO composites with different molar ratios were investigated at each optimum temperature. The results show that the In2O3/CdO composite with a molar ratio of 10:1 has excellent sensing properties: the response to 10x10(-6) HCHO is 13.6, the response/recovery time is 140 s/32 s, and the selectivity is better at a lower operating temperature of 200 degrees C. In addition, the HCHO-sensing mechanism of the sensors based on the In2O3/CdO composites was briefly analyzed.
What problem does this paper attempt to address?