Photoluminescence Properties of Y0.75−xGdxAl0.10BO3:Eu3+0.10, 0.05R3+(R= Sc, Bi) (0.00 ≤x≤ 0.45)

Li Jie,Wang Yu-Hua,Dong Qi-Zheng,Liu Ji-Di
DOI: https://doi.org/10.1088/1674-1056/19/6/063301
2010-01-01
Chinese Physics B
Abstract:Y0.75-xGdxAl0.10BO3:Eu-0.10(3+), 0.05R(3+) (R=Sc, Bi) (0.00 <= x <= 0.45) powder samples are prepared by solid-state reaction and their luminescence properties are investigated. With the replacement of Y3+ ions by Sc3+ (or Bi3+) and Gd3+ ions in (Y, Al)BO3:Eu, the intensities of emission at 254 and 147 nm are remarkably improved, because Sc3+ ions can absorb UV light and transfer the energy to Eu3+ ions efficiently. Moreover, Gd3+ and Bi3+ ions act as an intermediate "bridge" between the sensitizer and the activator (Eu3+) in energy transfer to produce light in the (Y, Gd)BO3:Bi3+, Eu3+ system more effectively. After doping an appropriate concentration of Gd3+ into Y0.50Gd0.25Al0.10BO3:Eu-0.01(3+), Bi-0.05(3+), the emission intensity reaches its maximum, which is nearly 110% compared with the red commercial phosphor (Y, Gd)BO3:Eu and better chromaticity coordinates (0.650, 0.350) are obtained.
What problem does this paper attempt to address?