Hot Deformation Behavior and Microstructure Evolution of Titanium Alloy Ti-Al-Zr-Sn-Mo-Si-Y

Qi Yun-Lian,Xi Zheng-Ping,Zhao Yong-Qing,Wang Rui-Ning,Du Yu,Luo Yuan-Yuan,Zeng Wei-Dong
IF: 3.752
2007-01-01
Transactions of Nonferrous Metals Society of China
Abstract:Samples of Ti-Al-Zr-Sn-Mo-Si-Y alloy were compressed on the Gleeble-1500 heat stimulation machine. The compression test was carried out in the temperature range from 800 degrees C to 1 100 degrees C and strain rate range from 0.001 s(-1) to 10 s(-1). Stress-strain behavior and variation of microstructure of the alloy during hot compression were investigated. The experimental results show that the alloy is sensitive to temperature and strain rate, and the flow softening behavior is more obvious with the decrease of deformation temperature. At higher strain rate, discontinuous yielding is observed in ss phase region. When deformed in alpha+ss phase region, with the increment of deformation temperature, the lamellar alpha structures globularization is more quick and more uniform. When deformed in ss phase region, coarse ss grains can be got because of high deformation temperature.
What problem does this paper attempt to address?