Mechanical Behavior of Fe75Mo5P10C7.5B2.5 Bulk-Metallic Glass under Torsional Loading

Xinjian Zhang,Lu Huang,Xu Chen,Peter K. Liaw,Ke An,Tao Zhang,Gongyao Wang
DOI: https://doi.org/10.1016/j.msea.2010.08.072
2011-01-01
Abstract:Pure- and cyclic-torsional studies were conducted on a Fe75Mo5P10C7.5B2.5 (atomic percent, at.%) bulk-metallic glass at room temperature for an understanding of its damage and fracture mechanisms. Under pure-torsional loading, the metallic glass exhibited very little plastic strain before fracture. The fracture initiated along the maximum tensile-stress plane, which is about 45 to the axial direction. The shear-fracture strength (similar to 510 MPa) is much lower than the compressive-fracture strength (similar to 3280 MPa), which suggests that different deformation mechanisms be present under various loading modes. Instead of an apparent vein-type structure, the fracture morphologies revealed a crack-initiation site, a mirror region, a mist region, and a hackle region. Under cyclic-torsional loading, fatigue cracks initiated from casting defects, and propagate generally along the maximum tensile-stress plane. A slight cyclic-hardening behavior was observed in initial loading steps. The fatigue-fracture surface consists of three main regions: the fatigue crack-initiation, crack-propagation, and final-fast-fracture areas. The striations resulting from the blunting and re-sharpening of the fatigue crack tip were observed in the crack-propagation region. Based on these results, the damage and fracture mechanisms of the metallic glass induced by torsional loadings are elucidated. (C) 2010 Elsevier B.V. All rights reserved.
What problem does this paper attempt to address?