Characteristics Of Perfluoroethane Thermal Decomposition

He Lin,Han Jun,Wang Guang-Hui,Heejoon Kim,Yao Hong
DOI: https://doi.org/10.3321/j.issn:0251-0790.2009.01.024
2009-01-01
Abstract:Perfluorocarbons (PFCs) gases have high global warming potential (GWP) and a long lifetime in the atmosphere. It is difficult to decompose these gases due to their tetrahedral structure arising from strong C-F bonds. This paper discussed C2F6 (one of PFCs gases) thermal decomposition characteristic under 950-1100 degrees C in a laboratory scale reactor. The effects of C2F6 initial concentration, reaction temperature, residence time on C2F6 decomposition ratio were also investigated. The experimental results indicate that the lower initial C2F6 concentration, higher reaction temperature, longer residence time can promote C2F6 decomposition ratio. On the basis of the results, it can be drawn that the reaction order of C2F6 thermal decomposition is between 0 and 1. Above 90% C2F6 decomposition ratio can be achieved under a temperature of 1100 degrees C, 223.21 mu mol/L initial C2F6 concentration and 2 s residence time. Basis on the calculation, the activation energy (E) and the frequency factor (A) of C2F6 thermal decomposition in the temperature range of 950-1100 degrees C were 313.2 kJ/mol and 8.8 x 10(11) s(-1), respectively.
What problem does this paper attempt to address?