pH Variation as Indicator for the Reaction between Arsenite and Absorbents

YE Ying,JI Shan-shan,WU Dai-dai,ZHANG Wei-rui
DOI: https://doi.org/10.3969/j.issn.1006-7493.2006.02.010
2006-01-01
Abstract:Three types of absorbents, ferric hydroxide, Mg-Al layered double oxide (Mg-Al-LDO) and Mg-Fe layered double oxide (Mg-Fe-LDO) were studied for their absorption behavior on arsenite. Initial pH value of NaAsO2 solution was 9.71. After ferric hydroxide being added, the pH variation with time can be divided into 3 stages: in the first 6 minutes, pH increased from 9.71 to 10.36, which indicates a OH-release from the solid phase into the solution; during 7 th ~ 40 th minutes, pH changed only a little between 10.36-10.34, which indicates absorption of ferric hydroxide on AsO2- and a dynamic equilibrium is reached; after 40 th minute, pH value decreased continuously to 9.72 at the 360 th minute, which is caused by condensation reaction between the arsenite and absorbent, and H+ is released as a result. During the absorption of Mg-Al-LDO on arsenite, pH values increased with time continuously, because Mg-Al-LDO takes anions from the solution to recover the crystal structure of its precursor, and in this reaction hydroxyl is formed. In the case of Mg-Fe-LDO, the absorption effects on arsenite for former two absorbents were observed, and pH-time curve is between these two absorbents. The absorption capacity of ferric hydroxide on arsenite changed a little with temperature, from 69.7 mg/g at 25℃ to 73.7 mg/g at 90℃. Absorption capacity of Mg-Al-LDO and Mg-Fe-LDO increased apparently when the medium was heated, from 62.4 mg/g and 82.5 mg/g at 25℃, to 114.9 mg/g and 199.0 mg/g at 90℃, respectively. Ascending absorption capacity of Mg-Al-LDO and Mg-Fe-LDO on arsenite at 90℃ is quite possibly because the disturbance of dissolved carbonic anion on arsenite is suppressed by heating, which expelled dissolved CO2 from the solution.
What problem does this paper attempt to address?