REINFORCEMENT OF NATURAL CELLULOSE WHISKER ON NATURAL RUBBER

Gu Ju,Li Xionghui,Jia Demin,Luo Yuanfang,Cheng Rongshi
DOI: https://doi.org/10.3724/sp.j.1105.2009.00595
2009-01-01
Acta Polymerica Sinica
Abstract:Cellulose whisker (CW) was prepared by hydrolysis of natural microcrystalline cellulose(MCC) with sulfate acid. The NR/CW composite was prepared by natural rubber (NR) latex coagulated with CW suspension. The results show CW has well reinforcement effect to NR. The modulus, elongation at break, tear strength of NR composites are further improved by using CW modified by resorcinol (R) and hexamethylene tetraamine (H) The mechanical properties of hot air aging (100 degrees C, 72 h) of NR/CW composite vulcanlizates are markedly superior to those of NR. The tensile strength of NR/RH-CW composites was dropped from 28.54 MPa to 21.78 MPa, the rate of change was down to 23.7%, and the elongation at break decreased from 594% to 493% and the change rate decreased to 17.0%. The tensile strength of pure NR was dropped from 22.02 MPa to 2.40 MPa, and the change rate was 89.1%; and the elongation at break was dropped from 579% to 168% and the change rate was 71.0%. SEM photo shows the interface compatibility between RH-CW and NR matrix was improved in comparison with CW and NR. TGA results show the 5% weight loss temperature of composites is decreased and the residue increases with CW adding. In addition, there is a peak of the derivative TGA curve at 520 degrees C, and the peak becomes larger and the residue increases with RH-CW adding.
What problem does this paper attempt to address?