Abstract:Co2-W type hexagonal ferrite was prepared by sol-gel method with metal nitrate as raw material,citrate as complexing agent and glycol as dispersive agent.TG-DTA,XRD and SEM were used to study the detailed information on the crystallography of the ferrite.The results showed that when calcination temperature was below 1200℃,the product is M-type ferrite.When calcination temperature was 1250~1300℃,the product was single W-type ferrite.A small amount of M-type ferrite is produced while calcination temperature was 1350℃.With extending the sintering holding time,W-type crystal is gradually purified.When holding time was 5h,a small amount of M-type ferrite were produced.Co2-W type ferrite was synthesized at calcination temperature 450℃ for 3h and 1250~1300 ℃ for 3h when the content of iron was 15.1.