Abstract:The photocarrier mobility of Fe 0.03wt%-doped potassium lithium tantalate niobate (K0.95Li0.05Ta0.61Nb0.39O3) was investigated by time-of-flight (TOF) measurement. The longitudinal photocarrier response due to pulsed excitation leads to values of the drift mobility of μh=1.45×10−2cm2/Vs for holes, μe=0.325×10−2cm2/Vs for electrons, and a value for the range of holes (μτ)h=4.38×10−5cm2/V at room temperature and at low field 3KV/cm. The response time of holes and electrons (or the relaxation time) is determined to be 3.02×10−3s and 3.74×10−3s, respectively. The mobility of holes strongly depends on the field strength, and is observed to decrease with increasing bias field.