MECHANISM OF INTERNAL FRICTION AND DIELECTRIC LOSS PEAKS OF Ce,Y-TZP CERAMICS

DU Juan,ZHENG Kai-yun,WAN Yi-ye,JIN Xue-jun
DOI: https://doi.org/10.3321/j.issn:1000-0542.2006.03.021
2006-01-01
Abstract:The room temperature(RT)~250℃ internal friction(IF) for quenched 8Ce,0.5Y-TZP ceramics and RT~400℃ dielectric loss(DL) for 8Ce,0.5Y-TZP and 8Ce,0.75Y-TZP ceramics were studied.Along with a relaxation peak,which is typical of normal 8Ce,0.5Y-TZP,two prominent IF peaks associated with phase transformation were observed in IF spectra for quenched 8Ce,0.5Y-TZP.The activation energy is discovered to be identical for both the mechanical and dielectric relaxation.More evidences are found that reorientation of Y_(Zr')V_ anisotropic complexes formed by oxygen vacancies and substitutional yttrium ions were confirmed to be the origin of the relaxation peak of Ce,Y-TZP ceramics.