Abstract:The hot ductility of 12CrMo continuously cast slabs used for mid-temperature pressure vessel steel was investigated on a Gleeble-3500 by means of tensile test,which was carried out at varying temperatures with a strain rate of 10-3 s-1.Fracture area reduction ratio was measured and microstructures and precipitates were examined.It is found that dynamic recrystallization occurs when specimens are deformed above 900 ℃,and thus the steel has good ductility with the area reduction ratio≥85%.A large amount of fine AlN is precipitated,the size being approximately 10 nm,when specimens are deformed at 850 ℃.A lot of proeutectiod ferrite grains form along austenite grain boundaries when specimens are deformed at 800 ℃,and consequently,the steel has poor hot ductility because the area reduction ratio is lowered to 36%.