Fluorescence and Attenuation Properties of Er 3+ -Doped Phosphate-Glass Fibers and Efficient Infrared-to-visible Up-Conversion

Y. -L. Lu,Y. -Q. Lu,N. -B. Ming
DOI: https://doi.org/10.1007/bf01080957
1996-01-01
Abstract:Fluorescence spectra of phosphate glasses with different erbium doping have been measured. The flourescence intensity reaches its maximum at an Er3+-doping concentration of 0.75 mol%. When the Er3+ doping exceeds 0.75 mol%, the fluorescence intensity decreases due to concentration quenching. The attenuation at 1.53 µm of the fiber is 12.8 db/m. The fluorescence up-conversion of 1.064 µm Nd:YAG laser pulses into intense green 547 and 667 nm light in the fiber has been measured. The fluorescence output power of green (547 nm) and red (667 nm) light is 178 and 42 μW, respectively with an excitation power of 1 W. The two signals are referred to as4S3/2 →4I1 5/2 and4F9/2 →4I1 5/2 transitions through two-photon absorption fluorescence.