Kinetic Study of the Delignification of Corn Stover by KOH Cooking

SUN Yong,ZHANG Jin-ping,YANG Gang,LI Zuo-hu
DOI: https://doi.org/10.3969/j.issn.1004-8405.2007.03.003
2007-01-01
Abstract:The corn stover which was pretreated with dilute chloride acid at 120℃ was cooked with KOH at 80, 90, 100 and 110℃, respectively. The delignification kinetic model of corn stover used three first order reactions with following form: WL=0.0137 exp(-∞t)+0.8433 exp(-k2t) +0.1430 exp(-k3t). The first term was essentially infinite at the time scale of cooking. The second and third terms corresponded to the bulk and residual phases of delignification. The activation energies for dilignification in cooking reaction were 54.46 and 27.62 kJ/mol in the bulk and residual phases, respectively. The optimal cooking condition was determined as following: cooking at 100℃ for 100 min. The delignification rate could be over 90%.