Beneficiation Experiment on Fluorite Recovery of Lead-Zinc Tailing from Hunan
Jiang Xiangwei,Guo Yanzhe,Liu Runqing,Jiang Wei,Liu Hang,Sun Wei
DOI: https://doi.org/10.3969/j.issn.1001-1250.2016.06.017
2016-01-01
Abstract:There is 18. 58% CaF2 in a lead-zinc mined tailings from Hunan,the main impurity composition is SiO2 and Ca-CO3 . In order to provide the basis of the fluorite recovery and utilization of tailings,beneficiation experiment was conducted on the ore. The results indicated that,CDG100 mm×100 mm cycle pulsating high intensity magnetic separator was used to remove iron, non magnetic products with Na2 CO3 as regulator,Na2 S and sodium silicate as inhibitor,acidification sodium silicate ( ratio of sul-phunic acid to sodium silicate is 2 ∶ 1) as depressor for cleaning,Z-202 as collector,by one roughing,seven cleaning,one scaven-ging closed circuit flotation test process,fluorite concentrate with CaF2 grade of 94. 76%,recovery rate is 53. 83% was obtained. Test results can provide technical guidance for comprehensive utilization of lead-zinc mined tailings containing fluorite.