The role of arsenic in the homogeneous precipitation of As, Sb and Bi impurities in copper electrolyte

Xue-Wen Wang,Qi-Yuan Chen,Zhou-Lan Yin,Ming-Yu Wang,Fang Tang
DOI: https://doi.org/10.1016/j.hydromet.2011.04.007
IF: 4.217
2011-01-01
Hydrometallurgy
Abstract:The role of arsenic in the homogeneous precipitation of impurities arsenic, antimony and bismuth in copper electrolyte was studied. Experiments found that though the formation of arsenato antimonates is one of the control-steps in the homogeneous precipitation and antimony is absolutely necessarily for arsenato antimonates formation, arsenic played an important role for the homogeneous precipitation as well. Arsenic (V) is not only a reactant of arsenato antimonates formation but also an oxidant of Sb(III) oxidation. Arsenic (V) can oxidize antimony from Sb(III) to Sb(V) in copper electrolyte. If the concentration of arsenic (V) is over 6g/L and the mole ratio of As(III)/As(V) is less than 0.09, the oxidation can be taken place at room temperature, and the equilibrium value of the φAs(V)/As(III) is about 0.606 in the electrolyte. Under these conditions, the precipitation rate of antimony from the electrolyte can be reached over 97%. Arsenic (III) can promote arsenato antimonates formation and depress floating slimes formation simultaneously. The higher the arsenic (III) concentration is, the easier the formation of arsenato antimonates will be. If arsenic (III) is lack, the copper electrolyte is prone to be over oxidized, which will result in the formation of floating slimes. Floating slimes and arsenato antimonates have a similar chemical composition. To distinguish arsenato antimonates from floating slimes, the most effective way was thermal decomposition.
What problem does this paper attempt to address?