Study on Bio-compatibility of PLGA/HA in Vivo

ZHANG Shi-jie,PEI Qing-guo,PAN Ke-feng,JIANG Xin-quan,ZHANG Xiu-li
DOI: https://doi.org/10.3969/j.issn.1005-4979.2007.01.010
IF: 1.9
2007-01-01
Journal of Oral and Maxillofacial Surgery
Abstract:Objective: To evaluate biological compatibility of a new porous polyaiticglycolic acid/hydroxyapatite(PLGA/HA) scaffold in animal experiment. Methods: PLGA/HA scaffold (with 5% HA or 10% HA) were injected into Kunming mice intraperitoneally and implanted into New Zealand rabbits. The biocompatibility experiments included systemic toxicity test, sub-acute toxicity test, blood compatibility test, and muscle stimulation test. Results: After injection and implantation of PLGA/HA scaffold into mice and rabbits, general condition of animals remained normal.Weight, red blood cell count, and white blood cell count of experimental animals altered slightly. Rabbit mixed plasma coagulation function wasn't affected. Hemolytic rate of PLGA/HA scaffold with 5% HA or 10% HA were 2.67% and 3.62% respectively, which met the requirement of hemolysis test standard (5%)as a medical material. Muscle stimulation test revealed that implantation did not cause any local redness. Part of PLGA/HA scaffold started to degrade at 4th week. There were little inflammatory cell infiltrations around the material 4 weeks after implantation. Conclusion: Both PLGA/HA scaffold with 5% HA or 10% HA have good biocompatibility.
What problem does this paper attempt to address?