Ferroelectric BaTiO3 Nanoceramics Prepared by a Three‐step High‐pressure Sintering Method

C. J. Xiao,W. W. Zhang,Z. H. Chi,F. Y. Li,S. M. Feng,C. Q. Jin,X. H. Wang,L. T. Li,R. Z. Chen
DOI: https://doi.org/10.1002/pssa.200622399
2007-01-01
Abstract:Dense BaTiO3 nanoceramics with a homogeneous grain size of 30 nm were prepared at 6 GPa, 1000 °C using a three‐step high‐pressure sintering method. The microstructure of the ceramics obtained is uniform and the relative density is above 98% of the theoretical value. Similar to normal BaTiO3 ceramics, successive phase transitions are observed in the 30 nm BaTiO3 ceramics using variable‐temperature X‐ray diffraction measurements. Furthermore the 30 nm BaTiO3 ceramics reveal ferroelectric properties after being post‐annealed at low temperature in O2 atmosphere, but the phase transition temperature from paraelectric to ferroelectric phase is 10 °C lower than that of a normal bulk sample. The results indicate that dense 30 nm BaTiO3 ceramics retain ferroelectricity above room temperature. (© 2007 WILEY‐VCH Verlag GmbH & Co. KGaA, Weinheim)
What problem does this paper attempt to address?