Enhancement of Rutile Formation by ZrO2 Addition in Ti-bearing Blast Furnace Slags
Zhongmin Li,Yongqi Sun,Lili Liu,Xidong Wang,Zuotai Zhang
DOI: https://doi.org/10.2355/isijinternational.55.1384
2015-01-01
ISIJ International
Abstract:China has approximately 50% of the total titanium reserve in the world. However, about 98% of titanium resource is in the form of vanadium-titanium magnetite ores, which is generally treated with blast furnace ironmaking process (BF process) to extract valuable elements (e.g. V, Fe) from iron ore concentrate. In this process, Ti element is concentrated into the molten slag and discharged into the slag pit, forming the typical Ti bearing blast furnace slag waste (Ti-BF slag) containing 22–25 wt.% TiO2. The deposition of such waste not only poses hazardous effects on environment but also is a great loss of titanium resource. Therefore, it is necessary to develop a utilization method to treat these Ti-BF slags and extract Ti element efficiently. During past decades, many methods have been developed to extract Ti from Ti-BF slags, such as acid leaching,3,4) alkaline molten salt method,5,6) carbide-chloride method7,8) and selective crystallization and phase separation (SCPS) method.9,10) Currently, SCPS method has been thought as one of the most promising methods, which can enrich Ti element into a selected crystalline phase, which makes the extraction of titanium become feasible. Rutile is regarded as an appropriate enriched phase for SCPS method because of its rod-shape structure, high density and high content of Ti.11,12) However, the rate of rutile formation is still not Enhancement of Rutile Formation by ZrO2 Addition in Ti-bearing Blast Furnace Slags