Microstructure and Mechanical Properties of FeAl Intermetallics Prepared by Mechanical Alloying and Hot-Pressing

Haixia Song,Yunxin Wu,Chuan'an Tang,Shuai Yuan,Qianming Gong,Ji Liang,宋海霞,吴运新,唐传安,袁帅,巩前明,梁吉
DOI: https://doi.org/10.1016/S1007-0214(09)70044-6
2009-01-01
Abstract:FeAl intermetallics were prepared by mechanical alloying and vacuum hot-pressing. The Fe-48 at.% Al powder was ball-milled for 3–12 h, producing a solid solution structure of Fe (Al) with trace Al (Fe). Subsequent vacuum annealing or hot-pressing introduced phase transformations into the FeAl (B <inf xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</inf> ) inter­ metallics and Al <inf xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</inf> O <inf xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">3</inf> inclusions. The hot-pressed FeAl intermetallics possess a high flexural strength of 831 MPa and a fairly good strain at break of 3.2%. The results show that the addition of 0.5 at.% B reduces the peak temperature for hot-pressing from 1180 °centigrade; to 1100 °centigrade, and increases the density of the compacts from 95% to 96.3%, but results in no significant improvement in the mechanical properties.
What problem does this paper attempt to address?