Heat Treatment Effects on Microstructure and Magnetic Properties of Mn–Zn Ferrite Powders

Ping Hu,Hai-bo Yang,De-an Pan,Hua Wang,Jian-jun Tian,Shen-gen Zhang,Xin-feng Wang,Alex A. Volinsky
DOI: https://doi.org/10.1016/j.jmmm.2009.09.002
IF: 3.097
2010-01-01
Journal of Magnetism and Magnetic Materials
Abstract:Mn–Zn ferrite powders (Mn0.5Zn0.5Fe2O4) were prepared by the nitrate–citrate auto-combustion method and subsequently annealed in air or argon. The effects of heat treatment temperature on crystalline phases formation, microstructure and magnetic properties of Mn–Zn ferrite were investigated by X-ray diffraction, thermogravimetric and differential thermal analysis, scanning electron microscopy and vibrating sample magnetometer. Ferrites decomposed to Fe2O3 and Mn2O3 after annealing above 550°C in air, and had poor magnetic properties. However, Fe2O3 and Mn2O3 were dissolved after ferrites annealing above 1100°C. Moreover, the 1200°C annealed sample showed pure ferrite phase, larger saturation magnetization (Ms=48.15emug−1) and lower coercivity (Hc=51Oe) compared with the auto-combusted ferrite powder (Ms=44.32emug−1, Hc=70Oe). The 600°C air annealed sample had the largest saturation magnetization (Ms=56.37emug−1) and the lowest coercivity (Hc=32Oe) due to the presence of pure ferrite spinel phase, its microstructure and crystalline size.
What problem does this paper attempt to address?