Thermal Analysis and Thermal Decomposition Kinetics of Polyester

陈曦,于钦学,任文娥,龙虹毓
DOI: https://doi.org/10.3969/j.issn.1009-9239.2009.03.013
2009-01-01
Abstract:Based on thermal analysis kinetics,differential scanning calorimetry(DSC) and thermogravimetric analysis(TGA) were employed to evaluate the thermal decomposition behaviors of two types of polyester(PET,a-PET and b-PET),in air atmosphere at a single heating rate of 10 ℃·min-1.The glass transition temperature(Tg),melting point temperature(Tm),crystal temperature(Tc),crystallinity and some other parameters were obtained through DSC curves.The results are shown as follows: The Tg of a-PET and b-PET is 80.70 ℃ and 93.81 ℃,respectively;the Tm is 261.41 ℃ and 260.31 ℃,respectively;Tc is 128.28 ℃ and 229.59 ℃,respectively;and the crystallinity is 27.76% and 31.17%,respectively.Moreover,the kinetic parameters like activation energy,reactive index and pre-exponential factor were calculated and analyzed with Freeman-Carroll method in every decomposition stage,respectively.The conclusions can be deduced that there are two main decomposition stages in different temperature sectors of thermal decomposition.The activation energy,reactive index and pre-exponential factor of a-PET are respectively 141.00 kJ/mol,0.65 and 4.97E+9 min-1;and those of b-PET are 167.13 kJ/mol,0.39,4.33E+11 min-1 individually during the first stage (340~445 ℃) of thermal decomposition.In the second stage(515~561 ℃) of thermal decomposition,the activation energy,reactive index and pre-exponential factor of a-PET are 106.48 kJ/mol 0.66 and 2.2E+6 min-1,respectively;and those of b-PET are 123.04 kJ/mol,0.70,1.05E+7 min-1 individually.
What problem does this paper attempt to address?