Thermal Decomposition of Flame-retarded High Impact Polystyrene

Wu Zhongwei,Jiao Qingjie,Zang Chongguang,Lan Hui
DOI: https://doi.org/10.14159/j.cnki.0441-3776.2008.12.006
2008-01-01
Chemistry
Abstract:The thermal decomposition process and decomposed products of high impact polystyrene(HIPS) were analyzed by using TGA-IR and Py-GC/MS,respectively.Moreover,the radical reaction mechanism of the degradation of HIPS was discussed.The degradation process of flame-retarded system of decabromdiphenyl ethane(DBDPE) and antimony trioxide(Sb_2O_3) and the flame-retarded mechanism of condensed phase and gas phase for flame-retarded HIPS were investigated.The results showed that the β-scission of HIPS happened in combustion mainly;a mass of smog was composed of styrene,toluene,α-methyl-styrene,ethylbenzene,butadiene and so on.The condensed phase was composed of the products of 1,3,5-triphenyl-benzene and other oligomers.At different temperature,the pyrolyzed products of flame-retarded HIPS were different,and the small molecular compounds evidently increased at high temperature.
What problem does this paper attempt to address?