Abstract:Lignin was extracted from white pine sawdust by organosolv-extraction using hot-compressed ethanol-water co-solvent. The optimum conditions for extracting lignin from the pine sawdust were found to be at 180 degrees C with ethanol-water solvent (1: 1 wt/wt), where the lignin yield attained ca. 26% with a purity of ca. 83%. The lignin under such conditions was oligomers with a broad molecular weights distribution: M-n of 537, M-w of 1150 and polydispersity of 2.14. Bio-based phenol-formaldehyde resol resins were synthesized using the resultant lignin as the replacement of petroleum-based phenol at varying ratios from 25 to 75 wt.% by condensation polymerization catalyzed by sodium hydroxide. Upon heating the lignin-phenol-formaldehyde resols could solidify with a main exothermic peak at around 150-175 degrees C, typical of the conventional phenolic resol resins, and a secondary peak at 135-145 degrees C. likely due to the exothermic reactions between the free formaldehyde with phenol or lignin to form methylophenols. The replacement of phenol with lignin at a large ratio deferred the curing process, and the introduction of lignin in the resin formula decreased the thermal stability of the resin, leading to a lowered decomposition temperature and a reduced amount of carbon residue at elevated temperatures. For practical applications, it is suggested that the replacement ratio of phenol with lignin be less than 50 wt.% The thermal stability can however be improved by purifying the lignin feedstock before the resin synthesis. (C) 2009 Elsevier Ltd. All rights reserved.
What problem does this paper attempt to address?