Blood compatibility of 316L stainless steel applied with silk peptide/chitosan polymeric coating

Li Xiao-yan,Jiang Rong-jing,Liu Jian-ping,Cao Mei-xun,Li Sheng,Zheng Ying,Jiang Liu-yue
DOI: https://doi.org/10.3321/j.issn:1673-8225.2008.23.021
2008-01-01
Abstract:BACKGROUND: Applying polymer materials with good histocompatibility as the coating scaffolds of the hearts, may promote the growth of endothelial cells, inhibit the excessive growth of smooth muscle cells and reduce the local inflammatory reaction. Thus polymer materials are effective to improve the repair of endothelial injury and reduce the occurrence of thrombosis. OBJECTIVE: To observe the blood compatibility of 316 L stainless steel with silk peptide/chitosan polymeric coating membrane. DESIGN, TIME AND SETTING: An observation experiment was performed at Institute of Plant Physiology and Ecology, Shanghai Institute of Life Sciences, Chinese Academy of Sciences between July 2006 and July 2007. MATERIALS: 316L stainless steel was produced by Zhangjiagang Xianke Medical Apparatus Co., Ltd (China); Silk peptide was produced by Institute of Plant Physiology and Ecology, Shanghai Institute of Life Sciences, Chinese Academy of Sciences (China); Chitosan was produced by Zhejiang Province Yuhuan Marine Biochemistry Co., Ltd (China). METHODS: By means of electrostatic self-assembly method, a kind of polymeric membrane was prepared with silk peptide and chitosan and then applied on the surface of 316L stainless steel. MAIN OUTCOME MEASURES: The dynamic clotting time, platelet adherence through scanning electron microscope and hemolysis ratio of the stainless steel were all detected before and after coating to test the blood compatibility of this polymeric membrane. RESULTS: The dynamic clotting time for 316L stainless steel coated with the polymer of silk peptide and chitosan remarkably prolonged compared to that with no coating. The adherence experience showed there were more blood platelets sticking on the surface of the bare stainless steel, and the platelets deformed; While some platelets were also found on the surface of the coated 316L, but the platelet deformation and the density of aggregation were obviously less than the bare stainless steel. The hemolysis rate of the coated steel was less than 5%, which suggested the silk peptide/chitosan polymeric coating was avirulent. CONCLUSION: Compared to the bare 316L stainless steel, the silk peptide/chitosan polymeric coating prolongs the activated coagulation time, alleviates the adherence and distortion of platelets, and enhances the blood compatibility of 316L base.
What problem does this paper attempt to address?