STUDY ON THE AGING WEAKNESS OF DOUBLE-WIRE MIG WELDED JOINT OF 2519 HIGH STRENGTH ALUMINUM ALLOY

Fan Chenglei,Yang Chunli,Cheng Shijun,Guo Xuming
DOI: https://doi.org/10.3969/j.issn.1001-1382.2005.11.005
2005-01-01
Abstract:Because the heat input quantity during double-wire MIG welding thick plates was great,the welded joint was in the high temperature state for a long period of time and the former solidified metal experienced an "involuntary" aging treatment,which mean that the weld metal had reached the "peak aging" or sub-"peak aging" already.Thus,the double-wire MIG welded joint of 2519 aluminum alloy in 20 mm thickness had the aging weakness problem.During the aging after the welding,there precipitated lots of hard and brittle θ phase which had the incoherence relation with the base metal,which reduce the lattice distortion and the strength of the welded seam.Thus,the welded joint presented "overaging" state.Besides,the θ phase continuously aggregated along the grain boundary,which also reduced the strength of the grain boundary and welded joint.
What problem does this paper attempt to address?