Abstract:Two kinds of hybrid silicone nitride(Si3N4) particles with binary particle size distribution,i.e.,(15μm+0.6μm),(3μm+0.6μm),were used to reinforce silicone rubber at the 65% total fillers content.The properties of filled silicone rubber were investigated as a function of relative content of the 0.6μm small particles(Ws).The results indicate that thermal conductivity and tensile strength reach the maximum values at Ws being 20%,25% for the(15μm+0.6μm) reinforced system,and 40%,15% for the(3μm+0.6μm) reinforced system,respectively;dielectric constants reduce to the lowest values at the Ws of 20% and 30%,respectively,and coefficient of thermal expansion reduces with increasing the Ws for the two systems.Furthermore,the Si3N4 particle size has the effect on the properties of silicone rubber.