Effects of W element on the microstructure, wear and cavitation erosion behavior of CoCrFeNiMnW x high entropy alloy coatings by laser cladding

D.T. Yu,T. Zhao,C.L. Wu,S. Zhang,C.H. Zhang,H.T. Chen,R. Wang
DOI: https://doi.org/10.1016/j.matchemphys.2024.129630
IF: 4.778
2024-06-21
Materials Chemistry and Physics
Abstract:CoCrFeNiMnW x ( x = 0, 0.5, 1, 1.5, 2) high entropy alloy (HEA) coatings were prepared on the surface of 304 stainless steel (304 SS) by laser cladding technology. The effects of W addition on the microstructure, microhardness, friction and wear properties, and cavitation erosion (CE) resistance of the coatings were thoroughly studied. The results show that the phase structure of the CoCrFeNiMnW x HEA coatings exhibits FCC structure, and the microstructure is typical dendrite (DR) and inter-dendrite (ID) morphology. With the increase of W content, the average grain size of CoCrFeNiMnW x HEA coatings gradually decreases. The microhardness of CoCrFeNiMnW x HEA coatings increases first and then decreases due to the brittle cracking caused by the excessive addition of W element. The wear resistance of CoCrFeNiMnW 1 HEA coating is the highest, and its wear rate is much lower than that of CoCrFeNiMn HEA coating without W addition. The wear mechanism of CoCrFeNiMnW x HEA coatings is mainly adhesive wear, abrasive wear and oxidation wear, and the fatigue wear mechanism appears on CoCrFeNiMnW 2 HEA coating. In addition, CoCrFeNiMnW 1 HEA coating displays the highest CE resistance, and its mass loss after CE in 3.5wt.%Nacl solution is lower than that of CoCrFeNiMn HEA coating. The appropriate addition of W element can effectively improve the resistance to wear and CE of CoCrFeNiMnW x HEA coatings, showing a great potential in improving the service lifespan of overflow parts in marine environment.
materials science, multidisciplinary
What problem does this paper attempt to address?