Effect of metakaolin and lime addition on geopolymerization of construction and demolition waste

Arvind Pathak,Sanjay Kumar,Vinay Kumar Jha
DOI: https://doi.org/10.1007/s11356-024-35234-1
2024-10-08
Abstract:Construction and demolition waste generates the largest amount of waste by volume, which threatens sustainable development and adversely affects the environment. These wastes contain a significant amount of aluminosilicates that have the potential to be used as building materials for value-added applications applicable to alternative construction materials. This study aims to synthesize geopolymers from brick powder using metakaolin/lime as additives and compare their physico-mechanical properties. The compressive strengths of the geopolymer products GP-1, GP-2, and GP-3 developed at 28 days from brick powder and metakaolin/lime with the activator solution were found to be 8.35, 21.30, and 25.0 MPa respectively, 2.55 and 2.99 times higher when metakaolin and lime were added. FTIR spectra and SEM-EDX micrographs of the reaction products showed structural changes and formation of aluminosilicate hydrate and calcium silicate hydrate gel with Al2O3/Na2O ratios of 0.75, 1.67, and 1.98 respectively. The reaction products containing SiO2/(SiO2 + Al2O3 + Fe2O3) ratios of 0.70 and 0.76 were found to be desirable. The geopolymer product GP-3 was found to have a higher bulk density and mechanical strength than those of GP-1 and GP-2. These products are found to be very hard, with potential applications in construction industries to conserve the environment.
What problem does this paper attempt to address?