Enhanced Degradation of Various Dyes Under Sunlight Using Hybrid Nanomaterials

Abraham Elmushyakhi,Faten Ismail Abou El Fadl,Abou El Fadl, Faten Ismail
DOI: https://doi.org/10.1007/s10904-024-03056-w
IF: 3.518
2024-03-31
Journal of Inorganic and Organometallic Polymers and Materials
Abstract:As the aim of all researcher in the field of water purification, is to develop new materials with high reactivity this study took the advance to apply the hybrid Ca(OH) 2 /Ag nanocomposite which is not used very often in this filed for the catalytic reduction of various types of dyes separately and in a mixture to assess their ability and effectiveness under contact with direct sunlight. The catalytic degradation of dyes was considered under various conditions: with and without adding reducing agent, and with and without applying sun light to evaluate the reductive ability of the catalyst under study at all conditions. The prepared Ca(OH) 2 /Ag hybrid nanocomposite, examined by XRD and TEM to study their morphology size and shape and to prove the presence of both nanoparticles Ca(OH) 2 and Ag and the results showed a high crystalline structure with an average particle size of 10.9 nm nanoparticles formed. The results of degradation of all dyes under test (acidic green dye 25 (AGD25), orange direct dye (ODD), and basic blue dye 41(BBD41)) showed that under applying the Ca(OH) 2 nanoparticles only the degradation percentage reached nearly 84, 67, 73.8% respectively, after 24 h. The primed nanocomposite Ca(OH) 2 /Ag exhibited an unusual ability to reduce all various tested dyes by using 0.2 g of prepared hybrid nanocatalyst, which was adequate to degrade a 50 ml solution of 200 mg/L concentration of each dye after nearly 60 min, this time differs somewhat with varying the type of dye where the degradation percentage reached 98, 90, and 97% for AGD25, ODD, and BBD41, respectively. The results revealed that the acid green 25 dye (AGD25) had the most significant degradation percentage compared with the other tested dyes, which grasped to 98% after only 60 min. Also, the degradation experiment carried out under various factors as initial concentration of dye, amount of catalyst, and temperature and the results showed that increasing the amount of catalyst and temperature enhances the degradation pf AGD25 to completion.
polymer science
What problem does this paper attempt to address?