Hardness and Corrosion Resistance of Low-Temperature Gas-Phase Carburization Coatings on Austenitic Stainless Steel after Pretreatments of Iron Electroplating or Fluorination

Zhang Liangjie,Pan Lin,Dong Gencheng,Yang Minhong,Li Peng
Abstract:Austenitic stainless steel has low hardness and poor service life, and the passivation film on its surface makes it hard to be carburized. Thus pre-treatments of iron electroplating and fluorination were conducted for austenitic stainless steel subjected to carburizing. After the surface passivation film was removed by pretreatments, the stainless steel was gas-phase carburized at a lowered temperature of 500 ℃. The hardness and corrosion resistance of as-obtained carburizing coatings were analyzed. Results show that fluorination as a pretreatment is more effective than iron electroplating in removing the passivation film on the stainless steel surface. The carburizing coatings formed on the stainless steel substrates after two kinds of pretreatments both have significantly increased hardness, meeting with the requirement of surface hardness of stainless structures between 600~800 HV. Besides, the carburizing coatings in relation to two kinds of pretreatments are both uniform and possess slightly improved corrosion resistance than the steel substrate.
Engineering,Materials Science
What problem does this paper attempt to address?