Influence of high concentration Zn2+ on floatability of sphalerite in acidic system

Ting-sheng QIU,Guo-dong LI,Xiao-bo LI,Hua-shan YAN,LIU Chen,Chen LIU
DOI: https://doi.org/10.1016/s1003-6326(21)65643-1
IF: 3.752
2021-07-01
Transactions of Nonferrous Metals Society of China
Abstract:The influence of high concentration Zn2+ on the floatability of sphalerite in an acidic system was investigated via flotation experiments, zeta potential measurements, contact angle measurements, and X-ray photoelectron spectroscopy. The results indicated that Zn2+ was adsorbed on the sphalerite surface and a Zn-hydroxyl complex was formed at a pH of 4 and a Zn2+ concentration of 4×10−2 mol/L. The zeta potential increased and the contact angle decreased from 84.80° to 36.48°, strongly inhibiting the floatability of sphalerite. When S2− or Cu2+ activator was used alone, sphalerite was not activated after Zn2+ was adsorbed, and its contact angle did not change significantly. However, by using a combination of S2− and Cu2+ activators, its floatability was realized after Zn2+ adsorption. This result was attributed to the removal of the Zn-hydroxyl complex on the surface of sphalerite by S2−. After this removal, Cu2+ was adsorbed on the sphalerite surface to form a Cu2S·S0 hydrophobic film.
metallurgy & metallurgical engineering
What problem does this paper attempt to address?
The paper primarily explores the impact of high concentrations of Zn²⁺ on the flotation behavior of sphalerite in an acidic environment and investigates the mechanism of activating inhibited sphalerite using a composite activator of Cu²⁺ and S²⁻. ### Research Background and Problem During the flotation process of zinc leaching residue, the presence of a large amount of zinc sulfate (ZnSO₄) in the slurry results in a pH value between 3 and 5. High concentrations of Zn²⁺ strongly inhibit the flotation of sphalerite. Using Cu²⁺ or S²⁻ alone as an activator cannot effectively activate sphalerite adsorbed with Zn²⁺. Therefore, it is necessary to study how to restore the flotation performance of sphalerite by adding an appropriate composite activator. ### Main Findings 1. **Flotation Experiment Results**: When the concentration of Zn²⁺ reaches 4×10⁻² mol/L, the recovery rate of sphalerite drops from 96.2% without Zn²⁺ to 55%, indicating that Zn²⁺ has a strong inhibitory effect on sphalerite. However, by adding a composite activator of Cu²⁺ and S²⁻, a recovery rate of 94.32% can be achieved. 2. **ζ Potential and Contact Angle Analysis**: High concentrations of Zn²⁺ adsorb on the surface of sphalerite, leading to an increase in ζ potential and a decrease in contact angle, making the sphalerite surface hydrophilic. Adding Cu²⁺ or S²⁻ alone cannot significantly change these properties, but using a combination of Cu²⁺ and S²⁻ results in a decrease in ζ potential and an increase in contact angle to 102.29°, indicating effective activation. 3. **X-ray Photoelectron Spectroscopy (XPS) Analysis**: Zn²⁺ exists on the surface of sphalerite in the form of metal hydroxyl complexes, hindering the adsorption of Cu²⁺ and making the surface hydrophilic. S²⁻ can effectively remove the Zn-hydroxyl complexes from the surface of sphalerite, promoting the adsorption of Cu²⁺ and forming a hydrophobic Cu₂S∙S₀ film. ### Conclusion 1. High concentrations of Zn²⁺ at pH=4 strongly inhibit the recovery of sphalerite. Using Cu²⁺ or S²⁻ alone is difficult to activate sphalerite, while the combination of Cu²⁺ and S²⁻ can achieve a recovery rate of 94.32%. 2. Zn²⁺ adsorption leads to an increase in ζ potential and a decrease in contact angle, while the combination of Cu²⁺ and S²⁻ results in a decrease in ζ potential and an increase in contact angle to 102.29°. 3. XPS analysis shows that Zn²⁺ exists in the form of metal hydroxyl complexes, and S²⁻ can remove these complexes and promote the adsorption of Cu²⁺, forming a hydrophobic film.