Exploiting synchrotron X-ray tomography for a novel insight into flax-fibre defects ultrastructure

Delphine Quereilhac,Lola Pinsard,Elouan Guillou,Marina Fazzini,Emmanuel De Luycker,Alain Bourmaud,Marwa Abida,Jonathan Perrin,Timm Weitkamp,Pierre Ouagne
DOI: https://doi.org/10.1016/j.indcrop.2023.116655
2023-03-31
Abstract:Flax fibres are valuable reinforcements for tomorrow's composites. However, defects called kink-bands, which mainly appear on fibres during the extraction and transformation phases, might affect their mechanical properties. Defects induced pores, within the kink-band are investigated in this work. They were morphologically explored using synchrotron phase-contrast X-ray microtomography, a technique that displays a sharp 3D representation of the pores. The study highlights the link between kink-bands and secondary cell wall ultrastructure. Pores are organised concentrically around the lumen, and their low thickness suggest that they are located at the interface between cellulose layers within S2 (G) layer. Moreover, the pores inclination with reference to the lumen axis follows the typical microfibrillar angle changes observed in the literature in the kink-band region. The volumes of the pores were measured, and a local increase in porosity was revealed in zones where defects are most severe along the fibre.
Applied Physics,Materials Science
What problem does this paper attempt to address?
The paper primarily explores structural defects in flax fibers—kink-bands—and their impact on the mechanical properties of the fibers. Specifically, the study focuses on the pore structure within the kink-band regions and uses synchrotron X-ray tomography to obtain 3D images of these pores. The main issues the paper attempts to address include: 1. **Pore organization and shape**: The study aims to reveal the specific organization, shape, and distribution of pores within the kink-bands. 2. **Relationship between pores and secondary cell walls**: It explores the connection between pores and secondary cell walls (particularly the S2(G) layer) to understand the reasons behind pore formation. 3. **Pore volume and defect severity**: It quantifies the pore volume and investigates its relationship with the severity of the kink-bands. 4. **Pore orientation and microfibril angle (MFA) changes**: It analyzes the correlation between pore orientation and changes in the microfibril angle. Through these studies, the authors hope to better understand the formation mechanisms of pores within kink-bands and how these pores affect the overall mechanical properties of flax fibers. This work is significant for improving flax fiber extraction processes and enhancing the performance of composite materials.