Hydrogen Embrittlement of a Prerolled High‐Mn Steel with Different Cut‐Edge Characteristics

Zhendong Sheng,Qihong Zheng,Mengya Wang,Yinghu Wang,Ulrich Prahl
DOI: https://doi.org/10.1002/srin.202400643
IF: 2.1258
2024-10-19
steel research international
Abstract:Hydrogen embrittlement behavior of a prerolled Fe–15Mn–0.65C–2Al–2Si high‐Mn steel with five cutting methods is investigated via hydrogen precharging and slow strain rate test. Corresponding fracture surfaces are linked to the cut‐edge properties and microstructures at cutting‐affected zones. The laser‐cut specimens show the highest tensile ductility while the blanked specimens show the lowest tensile elongation. Previous findings imply that mechanical twinning plays a critical role in transgranular cleavage features. The hydrogen embrittlement behavior of a prerolled Fe–15Mn–0.65C–2Al–2Si high‐Mn steel with various cut‐edge properties is studied via hydrogen precharging and slow strain rate test. In the presence of hydrogen, samples prepared by laser cutting under atmosphere of N2 exhibit the best total elongation at about 39%. Press blanking produces severe shear deformation, tensile residual stresses, and strain‐induced martensite, resulting in a high risk to hydrogen‐induced cracking. With compressive residual stresses produced from waterjet, corresponding samples exhibit the lowest elongation loss against hydrogen. Despite hydrogen charging, the fracture surfaces show transgranular quasi‐cleavage features, for which mechanical twinning from prerolling plays a critical role. The hydrogen‐enhanced decohesion mechanism accounts for cleavage fracture since hydrogen segregation reduces cohesive stress at twin boundaries.
metallurgy & metallurgical engineering
What problem does this paper attempt to address?