Realizing ranged performance in SnTe through integrating bands convergence and DOS distortion

Huimei Pang,Xiuxiu Zhang,Dongyang Wang,Rong Huang,Zhenzhong Yang,Xiao Zhang,Yuting Qiu,Li-Dong Zhao
DOI: https://doi.org/10.1016/j.jmat.2021.03.015
IF: 8.589
2022-01-01
Journal of Materiomics
Abstract:PbTe heavily alloying enhances the Seebeck coefficients of SnTe at high temperature range using bands convergence.Then, In was introduced to further enlarge Seebeck coefficients of SnTe at low-medium temperature range through utilizing DOS distortion.(Sn<sub>0.6</sub>Pb<sub>0.4</sub>)<sub>0.995</sub>In<sub>0.005</sub>Te achieves a notably high <em>ZT</em><sub>ave</sub> up to ∼ 0.67 over the wide temperature of 300 to 823 K.As a typical IV-VI compound, SnTe has aroused widely attentions in the thermoelectric community due its similar crystal and band structures with PbTe. However, both the large number of inherent Sn vacancies and high thermal conductivity result in inferior thermoelectric performance in intrinsic SnTe over a broad temperature. In this work, we successfully improved those disadvantages of SnTe <em>via</em> stepwisely Pb heavily alloying and then In doping. A significantly wide fraction of Pb into SnTe (0-50%) achieves multiple effects: (a) the carrier concentration of SnTe is reduced through decreasing Sn vacancies <em>via</em> alloying high solution Pb atoms in the matrix; (b) the band structure is optimized through promoting the convergence of the two valance bands, simultaneously enhancing the Seebeck coefficient; (c) HAADF-STEM coupled with EDS results illustrate that guest Pb atoms randomly and uniformly occupied Sn atomic sites in the matrix, concurrently strengthening the phonon scattering. Furthermore, we introduced indium into Sn<sub>0.6</sub>Pb<sub>0.4</sub>Te system to create resonant states further enlarging the power factors at low-medium temperature. The integration of bands convergence and DOS distortion achieves a considerably high <em>ZT</em><sub>ave</sub> of ∼ 0.67 over the wide temperature range of 300 to 823 K in (Sn<sub>0.6</sub>Pb<sub>0.4</sub>)<sub>0.995</sub>In<sub>0.005</sub>Te sample.<span class="display"><span><ol class="links-for-figure"><li><a class="anchor download-link u-font-sans" href="https://ars.els-cdn.com/content/image/1-s2.0-S2352847821000630-ga1_lrg.jpg"><span class="anchor-text">Download : <span class="download-link-title">Download high-res image (152KB)</span></span></a></li><li><a class="anchor download-link u-font-sans" href="https://ars.els-cdn.com/content/image/1-s2.0-S2352847821000630-ga1.jpg"><span class="anchor-text">Download : <span class="download-link-title">Download full-size image</span></span></a></li></ol></span></span>
materials science, multidisciplinary,chemistry, physical,physics, applied
What problem does this paper attempt to address?