Valorization of Sugarcane Leaf to Binderless Fiberboards by Hot‐Pressing Process and Polyurethane Coating

Watchara Sutaro,Jirapat Sarattawipak,Tanakorn Phuengklay,Pasakorn Kupasittirat,Sutipol Prommachan,Punyanich Intharapat,Natthapong Phinichka,Akarin Boonsombuti,Chantaraporn Phalakornkule
DOI: https://doi.org/10.1002/ceat.202400064
IF: 2.2148
2024-06-10
Chemical Engineering & Technology
Abstract:Binderless fiberboards were made with sugarcane leaf with <3 % moisture (w/w) and <1 mm in size by hot‐pressing temperature in the 210–240 °C range. An optimal pressing condition was 230 °C for pressing temperature, 5 MPa for pressing pressure, and 600 s for pressing time, giving 1200 kg m−3 for board density, modulus of elasticity of 657.1 MPa, modulus of rupture of 7.04 MPa, and internal bonding strength of 0.277 MPa. Sugarcane (Saccharum officinarum L.) leaf is an abundant waste from agriculture. In this study, we prepared binderless fiberboards from sugarcane leaf with <3 % moisture (w/w) and <1 mm in size by hot‐pressing temperature in the 210–240 °C range, followed by surface coating with polyurethane. The effect of hot‐pressing temperature on the modulus of elasticity (MOE), modulus of rupture (MOR), internal bonding (IB) strength, and thickness swelling of the binderless sugarcane leaves was investigated. An optimal pressing condition for preparing the binderless sugarcane leaf fiberboards was 230 °C for pressing temperature, 5 MPa for pressing pressure, and 600 s for pressing time, giving 1200 kg m−3 for board density, MOE of 657.1 MPa, MOR of 7.04 MPa, and IB strength of 0.277 MPa. The thickness swelling of the coated samples was almost completely eliminated by the surface coating.
engineering, chemical
What problem does this paper attempt to address?