Abstract:The H 2 production and self-assembly CNTs over Ni-Fe/Ni foam catalyst were investigated at different temperatures during steam reforming of bio-oil model compound. The formation of CNTs, CNFs and amorphous carbon and their different effects on catalytic activity were analyzed. With the temperature increasing from 500 °C to 800 °C, the amount of carbon deposition firstly increased and then decreased. It showed the highest amount of carbon deposition and largest proportion of CNTs (over 60 %) at 600 °C. The average diameter of CNTs was 15.18 nm. By contrast, more than 70 % of carbon deposition was amorphous carbon, and the CNFs with larger diameter (over 100 nm) were formed at 700 °C, which attributed to the agglomeration of metal particles at high temperature. The high reaction temperatures increased H 2 yield and pyrrole conversion, but differently, those at 600 °C was remarkably higher than that at 700 °C. It revealed that tip-growth of CNTs at 600 °C performed the self-activation effect to increase the catalytic activity, while the amorphous carbon generated at 700 °C deactivated the catalyst. After the reaction at 600 °C, the self-assemble of foam material showed the highest electrochemistry performance.
energy & fuels,engineering, chemical