Utilization of low metamorphic degree bituminous coal in direct reduction of high-phosphorus oolitic hematite and its mechanism

Kexin Yu,Wenjie Zou,Jue Kou,Chunbao Sun,Hongda Xu,Hao Dong,Bo Rao,Tichang Sun
DOI: https://doi.org/10.1016/j.fuel.2024.132497
IF: 7.4
2024-11-01
Fuel
Abstract:Coal-based direct reduction of high-phosphorus oolitic hematite is an effective method to realize the utilization of this kind of refractory iron ore resources with huge reserves. The performance of YJL bituminous coal with low metamorphic degree was compared with JS anthracite as reductants in the process of iron extraction and phosphorus removal of high-phosphorus oolitic hematite using the technique of direct reduction-magnetic separation. The mechanisms of reduction roasting and beneficiation of high-phosphorus oolitic hematite were studied employing X-ray diffraction (XRD) and scanning electron microscope-energy dispersive spectroscopy (SEM-EDS) and thermogrvimetric-differential scanning calorimetry analysis (TG-DSC). Results showed that the reduction results using these two reductants were comparable. For treating the raw ore with total iron (TFe) grade of 50.49 % and phosphorus content of 1.35 %, the direct reduced iron (DRI) with TFe grade of 93.97 %, TFe recovery of 86.14 % and phosphorus content of 1.20 % were obtained using 30 % YJL bituminous coal. The corresponding indexes using 30 % JS anthracite were 94.58 %, 86.15 % and 1.25 %, respectively. When 30 % limestone and 30 % YJL bituminous coal were added, the DRI with phosphorus content of 0.062 %, TFe grade of 94.51 % and TFe recovery of 87.47 % were obtained. The iron minerals were proved to be reduced following the sequence of Fe2O3 → Fe3O4 → FeO (Fe2SiO4, FeAl2O4) → Fe. The iron particles generated using YJL bituminous coal as reductant were smaller and more dispersed, they can still be recovered by grinding and magnetic separation. From TG-DSC, the total weight loss of YJL bituminous coal and JS anthracite were 33.97 % and 12.63 %, respectively. YJL bituminous coal and JS anthracite occurred depolymerization and decomposition reactions at 350 °C and 400 °C, respectively, producing and releasing a large amount of volatiles substances. YJL bituminous coal releases more reducing gases, mainly including H2, gaseous hydrocarbons and CO. And below 820 °C, the mixture of YJL bituminous coal and high-phosphorus oolitic hematite has a higher weight loss at 16.9 % than that of JS anthracite (7.86 %), indicating that YJL bituminous coal was more reactive to high-phosphorus oolitic hematite than JS anthracite at this stage. This work provided an effective utilization method for low metamorphic degree bituminous coal.
energy & fuels,engineering, chemical
What problem does this paper attempt to address?