Tensile Properties and Coefficient of Thermal Expansion of Laser Powder Bed Fusion Fabricated IN718‐YSZ Compositionally Graded Composite

Amey Parnaik,Jitendar Kumar Tiwari,Vijayavarman Chakkravarthy,Yaojie Wen,Baicheng Zhang,Ramasubramanian Lakshmi Narayan
DOI: https://doi.org/10.1002/adem.202401479
IF: 3.6
2024-10-06
Advanced Engineering Materials
Abstract:The addition of YSZ to IN718 via laser powder bed fusion is reported to lower the coefficient of thermal expansion of the composite and potentially reduce the thermal strain between the IN718 component and the YSZ thermal barrier coating. However, only IN718 with 2 wt% YSZ contain significant porosity (>2%) and solidification cracks, which reduces their strength and ductility significantly. In the section with 1.5 wt% YSZ, the YS, UTS, and ductility are 819 ± 30, 1008 ± 40, and 7.4 ± 0.4 MPa, which matches well with that of LPBF fabricated YSZ‐free IN718. Dilatometry measurements on sections with 0.5–1.5 wt% YSZ in the temperature range of 25–1200 °C indicate that their coefficient of thermal expansion (CTE) is intermediate to that of IN718 and YSZ. Finally, the variations in CTE with temperature are discussed in detail by considering the microstructural evolution in the composite with changes in temperature.
materials science, multidisciplinary
What problem does this paper attempt to address?