Large-Scale Electric-Field Confined Silicon with Optimized Charge-Transfer Kinetics and Structural Stability for High-Rate Lithium-Ion Batteries
Tao Meng,Bo Li,Qiushi Wang,Junnan Hao,Binbin Huang,Feng Long Gu,Huimin Xu,Peng Liu,Yexiang Tong
DOI: https://doi.org/10.1021/acsnano.0c01796
IF: 17.1
2020-05-13
ACS Nano
Abstract:The stereospecific design of the interface effects can optimize the electron/Li-ion migration kinetics for energy-storage materials. In this study, an electric field was introduced to silicon-based materials (C-SiO<sub><i>x</i></sub>@Si/rGO) through the rational construction of multi-heterostructures. This was achieved by manipulating the physicochemical properties at the atomic level of advanced Li-ion batteries (LIBs). The experimental and density functional theory calculations showed that the unbalanced charge distribution generated a large potential difference, which in turn induced a large-scale electric-field response with a boosted interfacial charge transfer in the composite. The as-prepared C-SiO<sub><i>x</i></sub>@Si/rGO anode showed advanced rate capability (<i>i</i>.<i>e</i>., 1579.0 and 906.5 mAh g<sup>–1</sup> at 1000 and 8000 mA g<sup>–1</sup>, respectively) when the migration paths of the Li-ion/electrons hierarchically optimized the large electric field. Furthermore, the C-SiO<sub><i>x</i></sub>@Si/rGO composite with a high SiO<sub><i>x</i></sub>@Si mass ratio (73.5 wt %) demonstrated a significantly enhanced structural stability with a 40% volume expansion. Additionally, when coupled with the LiNi<sub>0.8</sub>Co<sub>0.1</sub>Mn<sub>0.1</sub>O<sub>2</sub> (NCM) cathode, the NCM//C-SiO<sub><i>x</i></sub>@Si/rGO full cell delivers superior Li-ion storage properties with high reversible capacities of 157.6 and 101.4 mAh g<sup>–1</sup> at 500 and 4000 mA g<sup>–1</sup>, respectively. Therefore, the electric-field introduction using optimized electrochemical reaction kinetics can assist in the construction of other high-performance LIB materials.The Supporting Information is available free of charge at <a class="ext-link" href="/doi/10.1021/acsnano.0c01796?goto=supporting-info">https://pubs.acs.org/doi/10.1021/acsnano.0c01796</a>.Additional experimental data, including the FTIR spectrum of SiO<sub><i>x</i></sub>@Si, β-CD, and β-CD/SiO<sub><i>x</i></sub>@Si; SEM of SiO<sub><i>x</i></sub>@Si and SiO<sub><i>x</i></sub>@Si/rGO; TEM with SEAD of SiO<sub><i>x</i></sub>@Si and SiO<sub><i>x</i></sub>@Si/rGO; XPS of different samples; EPR of different samples; SEM of the SiO<sub><i>x</i></sub>@Si electrode after cycling; Raman spectra of the C-SiO<sub><i>x</i></sub>@Si/rGO electrode after cycling; schematic illustration of the evolution of SiO<sub><i>x</i></sub>@Si and C-SiO<sub><i>x</i></sub>@Si/rGO electrodes during cycling; schematic diagram of the configuration of the full cell and the prelithiated process, and the electrochemical performance of different electrodes (<a class="ext-link" href="/doi/suppl/10.1021/acsnano.0c01796/suppl_file/nn0c01796_si_001.pdf">PDF</a>)This article has not yet been cited by other publications.
materials science, multidisciplinary,chemistry, physical,nanoscience & nanotechnology