Boron‐polymer composites engineered for compression molding, foaming, and additive manufacturing

John R. Stockdale,Shelbie A. Legett,Xavier M. Torres,Adam Pacheco,Santosh Adhikari,Lindsey Bezek,Andrea Labouriau
DOI: https://doi.org/10.1002/app.55236
IF: 3
2024-01-31
Journal of Applied Polymer Science
Abstract:Diverse manufacturing techniques were employed to fabricate 3D printed pads, flexible foams and cast samples containing up to 80 wt.% boron. Boron (specifically 10B) is the element of choice to shield thermal neutrons due to its large (n, α) cross‐section; however, very few polymer composites containing high boron concentrations are available. This study aimed to determine the maximum possible amount of boron that could be introduced into a polymer matrix. Diverse manufacturing techniques, ranging from additive manufacturing to compression molding, were employed to fabricate inks and filaments for 3D printing, foams, and flexible pads. Composites using siloxanes, poly(lactic acid), and acrylonitrile butadiene styrene containing up to 80 wt% boron were sucessufully fabricated. The addition of known plasticizers (polyethylene glycol) and reinforcing agents (carbon nanofibers and fumed silica) helped to overcome fabrication problems such as clogging of the printing nozzle or crumbling of compression molded parts. In addition, the thermal‐mechanical properties of these novel boron composites were determined and shown to vary according to boron concentration, presence of additives, and fabrication techniques utilized.
polymer science
What problem does this paper attempt to address?